General
Property | Value |
---|---|
Densidad | 7.9 g/cm³ Show Supplier Material materials with Densidad of 7.9 g/cm³ |
Mecánica
Property | Value |
---|---|
Dureza Rockwell C | 59 - 65 [-] Show Supplier Material materials with Dureza Rockwell C of 59 - 65 [-] |
Módulo elástico | 230 GPa Show Supplier Material materials with Módulo elástico of 230 GPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 430 J/(kg·K) Show Supplier Material materials with Calor específico of 430 J/(kg·K) | |
Conductividad térmica | 20 °C | 22 W/(m·K) Show Supplier Material materials with Conductividad térmica of 22 W/(m·K) |
Eléctrico
Property | Value |
---|---|
Resistividad eléctrica | 5.3e-07 Ω·m Show Supplier Material materials with Resistividad eléctrica of 5.3e-07 Ω·m |
Chemical properties
Property | Value |
---|---|
Carbono | 1.35 % Show Supplier Material materials with Carbono of 1.35 % |
Cromo | 4.1 % Show Supplier Material materials with Cromo of 4.1 % |
Hierro | Balance |
Molibdeno | 5 % Show Supplier Material materials with Molibdeno of 5 % |
Vanadio | 4.1 % Show Supplier Material materials with Vanadio of 4.1 % |
Wolframio | 6 % Show Supplier Material materials with Wolframio of 6 % |
Technological properties
Property | ||
---|---|---|
Application areas | Thread-cutting tools, reamers, heavy-duty milling cutters, drills, punching tools |