General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.75 g/cm³ Show Supplier Material materials with Densidad of 1.75 g/cm³ | ISO 1183 |
Water content | 23.0 °C | 0.2 % Show Supplier Material materials with Water content of 0.2 % | ISO 15512 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 1.5 % Show Supplier Material materials with Elongación of 1.5 % | ISO 527-2 (5mm/min) |
Módulo de flexión | 23.0 °C | 12 GPa Show Supplier Material materials with Módulo de flexión of 12 GPa | ISO 178 (2mm/min) |
Módulo elástico | 23.0 °C | 12.5 GPa Show Supplier Material materials with Módulo elástico of 12.5 GPa | ISO 527-2 (1mm/min) |
Resistencia a la flexión | 23.0 °C | 250 MPa Show Supplier Material materials with Resistencia a la flexión of 250 MPa | ISO 178 (2mm/min) |
Resistencia a la tracción | 23.0 °C | 175 MPa Show Supplier Material materials with Resistencia a la tracción of 175 MPa | ISO 527-2 (5mm/min) |
Resistencia al choque, ensayo Charpy entallado | 23.0 °C | 13 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 13 kJ/m² | ISO 179/1eA |
Resistencia al choque, ensayo Charpy no entallado | 23.0 °C | 65 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 65 kJ/m² | ISO 179/1eU |
Resistencia al choque, ensayo Izod entallado | 23.0 °C | 12 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod entallado of 12 kJ/m² | ISO 180/1A |
Resistencia al choque, ensayo Izod no entallado | 23.0 °C | 60 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Izod no entallado of 60 kJ/m² | ISO 180/1U |
Aplicaciones térmicas
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Contenido de cenizas | 23.0 °C | 40 % Show Supplier Material materials with Contenido de cenizas of 40 % | ISO 3451-4 | ||
Heat deflection temperature, 0.45 MPa | 215 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 215 °C | ISO 75-2/B | |||
Heat deflection temperature, 1.80 MPa | 205 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 205 °C | ISO 75-2/A | |||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | ISO 3146 | |||
Ball Pressure Test | <2, for 125+/-2°C, EN 60695-10-2 | ||||
Inflamabilidad | UL94 (0.8mm) V0, EN 60695-11-10 |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Surface resistivity | 23.0 °C | 1.00E+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1.00E+14 Ω/sq | ASTM D257 |
Índice de seguimiento comparativo | 23.0 °C | 250 V Show Supplier Material materials with Índice de seguimiento comparativo of 250 V | EN 60112 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Halogenated, compliance with RoHS derivatives, with rating UL94 V0 and glow-wire at 960°C, which is used in many sectors of industy and has excellent mechanical properties. | |
Certifications | RoHS | |
Fillers | 40% Glass Fiber | |
Other | Laboratory conditions are 23 ±2°C and 45-55 % RH. |