Polyamide 66 (PA66)
Zytel® 70G30HSLR BK099Mezcla de polímeros
Crastin® LW9030 NC010Tereftalato de polibutileno (PBT)
Crastin® SK609 NC010Tereftalato de polibutileno (PBT)
Crastin® SK608 BK509Polyamide 66 (PA66)
RADIFLAM A RV250 AF 375 BKSuministrada por:
RadiciGroup High Performance PolymersPolyamide 66 (PA66)
RADIFLAM A RV350 AF 868 BRSuministrada por:
RadiciGroup High Performance Polymers