Módulo de flexión: 12 GPa

Quick Comparison

Polyamide 66 (PA66)

Zytel® 70G43L NC010

Polyamide 6 (PA6)

Akulon® K224-HG8

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® 46HF4540

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

LNP™ KONDUIT™ Compound PX13322

Suministrada por:

Sabic

Polyamide 6 (PA6)

LNP™ KONDUIT™ Compound PX13012

Suministrada por:

Sabic

Polietileno tereftalato (PET)

Rynite® 940 NC010

Polyamide 46 (PA46)

Stanyl® MC51

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

EPLAMID 6 GV0 40 NC Q1E0C001 (PA6)

Suministrada por:

EPSAN

Polyamide 4T (PA4T)

ForTii® MX15HR

Suministrada por:

DSM Engineering Materials

Other Polyamide (PA)

Akulon® GA-XLG0

Suministrada por:

DSM Engineering Materials

Polyamide 66 (PA66)

EPLAMID 66 GCF 30 BK Q1C0B001 (PA66)

Suministrada por:

EPSAN

Polyamide 6 (PA6)

EPLAMID 6 GFR 45 NC Q1E501 (PA6)

Suministrada por:

EPSAN

Polietileno tereftalato (PET)

Rynite® RE5264 NC010

Polyamide 46 (PA46)

Stanyl® TW271B3

Suministrada por:

DSM Engineering Materials

Éter de polifenileno (PPE)

LNP™ STAT-KON™ Compound ZE004

Suministrada por:

Sabic

Polieterimida (PEI)

LNP™ THERMOCOMP™ Compound EC004XXC

Suministrada por:

Sabic

Polyamide 46 (PA46)

Stanyl® TW278F10

Suministrada por:

DSM Engineering Materials

Other Polyamide (PA)

Stanyl® TC170

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® K224-G8U

Suministrada por:

DSM Engineering Materials
Página 1 de 2