General
Property | Value |
---|---|
Densidad aparente | 3.55 g/cm³ Show Supplier Material materials with Densidad aparente of 3.55 g/cm³ |
Porosidad | 4.0 % Show Supplier Material materials with Porosidad of 4.0 % |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 99.5 % Show Supplier Material materials with Aluminio of 99.5 % | Al₂O₃ |
Calcio | 0.02 % Show Supplier Material materials with Calcio of 0.02 % | CaO |
Hierro | 0.08 % Show Supplier Material materials with Hierro of 0.08 % | Fe₂O₃ |
Otro | 0.025 Show Supplier Material materials with Otro of 0.025 | max. Magnetic Iron |
Silicona | 0.04 Show Supplier Material materials with Silicona of 0.04 | SiO₂ |
Sodio | 0.04 - 0.3 % Show Supplier Material materials with Sodio of 0.04 - 0.3 % | Na₂O | for Alfa tab 06 | alfa tab 30 respectively |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Tabular Alumina is a raw material used in the manufacture of high alumina refractories, kiln furniture, electrical insulators, catalyst support media, investment casting, and more. |