General
Property | Value | Comment |
---|---|---|
Densidad | 5.6 g/cm³ Show Supplier Material materials with Densidad of 5.6 g/cm³ | |
5.7 g/cm³ Show Supplier Material materials with Densidad of 5.7 g/cm³ | ||
Densidad aparente | 1.2 - 1.3 g/cm³ Show Supplier Material materials with Densidad aparente of 1.2 - 1.3 g/cm³ | ANSI B74.4 |
Mecánica
Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de fusión | 2550.0 °C Show Supplier Material materials with Temperatura de fusión of 2550.0 °C |
Chemical properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Aluminio | 0.8 % Show Supplier Material materials with Aluminio of 0.8 % | ANSI B74.14 | Al₂O₃ |
Calcio | 3.8 % Show Supplier Material materials with Calcio of 3.8 % | ANSI B74.14 | CaO |
Circonio | 94.85 % Show Supplier Material materials with Circonio of 94.85 % | ANSI B74.14 | ZrO₂+HfO₂ |
Hierro | 0.05 % Show Supplier Material materials with Hierro of 0.05 % | ANSI B74.14 | Fe₂O₃ |
Silicona | 0.4 % Show Supplier Material materials with Silicona of 0.4 % | ANSI B74.14 | SiO₂ |
Titanio | 0.1 % Show Supplier Material materials with Titanio of 0.1 % | ANSI B74.14 | TiO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Fused Calcia-Stabilized Bubble Zirconia is used in the production of lightweight refractory bricks and castables, as loose bulk backup insulation for high temperature induction and nitriding furnaces, and other applications that require high temperature usage, rapid heating and cooling, and chemical stability. | |
Color | Yellow | |
Crystal structure | Cubic & Monoclinic Mixture | |
Other | Various sizes available. Custom sizes are also availble upon request. |