Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.1 Show Supplier Material materials with Aluminio of 0.1 | max. Al₂O₃ |
Circonio | 99 % Show Supplier Material materials with Circonio of 99 % | min. ZrO₂ |
Hierro | 0.04 Show Supplier Material materials with Hierro of 0.04 | max. Fe₂O₃ |
Silicona | 0.1 Show Supplier Material materials with Silicona of 0.1 | max. SiO₂ |
Titanio | 0.13 Show Supplier Material materials with Titanio of 0.13 | max. TiO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Fused Monoclinic Zirconia Powder is excellent in metallurgical refractories such as zirconia nozzles and slide gates. It is also used in other refractories, ceramic pigments, auto brake additives, setting sands, and more. | |
Other | Particle size: Hollow Spheres or Customized |