General
Property | Value | Comment |
---|---|---|
Densidad aparente | 0.9500000000000001 g/cm³ Show Supplier Material materials with Densidad aparente of 0.9500000000000001 g/cm³ | |
Rango de tamaño de partículas | 60.0 - 80.0 µm Show Supplier Material materials with Rango de tamaño de partículas of 60.0 - 80.0 µm | average |
Sieve residue 63μm | 20 % Show Supplier Material materials with Sieve residue 63μm of 20 % | |
50 % Show Supplier Material materials with Sieve residue 63μm of 50 % | ||
Área superficial específica | 4.0 - 8.0 m²/g Show Supplier Material materials with Área superficial específica of 4.0 - 8.0 m²/g | BET |
Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de fusión | 2000.0 °C Show Supplier Material materials with Temperatura de fusión of 2000.0 °C |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 99.7 % Show Supplier Material materials with Aluminio of 99.7 % | min. Al₂O₃ |
Calcio | 0.06 Show Supplier Material materials with Calcio of 0.06 | max. CaO |
Hierro | 0.05 Show Supplier Material materials with Hierro of 0.05 | max. Fe₂O₃ |
Silicona | 0.05 Show Supplier Material materials with Silicona of 0.05 | max. SiO₂ |
Sodio | 0.05 Show Supplier Material materials with Sodio of 0.05 | max. Na₂O |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Calcined Alumina is used in refractory applications as well as ceramic applications including spark plugs, tap washers, pump seal, electronic substrates, grinding media, abrasion resistant tiles, cutting tools, bioceramics, body armor, laboratory ware, and wear parts for the textile and paper industries. It is also used as a friction material in brake linings, in potting compounds to disperse heat, and in polishing, lapping, and buffing compounds. |