Property | Value | Comment |
---|---|---|
Densidad relativa | 3.8 [-] Show Supplier Material materials with Densidad relativa of 3.8 [-] | |
Loss on Ignition | 0.1 % Show Supplier Material materials with Loss on Ignition of 0.1 % | max. |
Rango de tamaño de partículas | 2.0 - 120.0 µm Show Supplier Material materials with Rango de tamaño de partículas of 2.0 - 120.0 µm | different specifications, please refer to the table below |
Tamaño de partícula D50 | 1.0 - 125.0 μm Show Supplier Material materials with Tamaño de partícula D50 of 1.0 - 125.0 μm | different specifications, please refer to the table below |
Área superficial específica | 0.02 - 1.2 m²/g Show Supplier Material materials with Área superficial específica of 0.02 - 1.2 m²/g | BET, different specifications, please refer to the table below |
Eléctrico
Property | Value |
---|
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 99.8 % Show Supplier Material materials with Aluminio of 99.8 % | min. Al₂O₃ |
Hierro | 0.02 Show Supplier Material materials with Hierro of 0.02 | Fe₂O₃ |
Silicona | 0.05 Show Supplier Material materials with Silicona of 0.05 | SiO₂ |
Sodio | 0.005 Show Supplier Material materials with Sodio of 0.005 | Na⁺ |
0.02 Show Supplier Material materials with Sodio of 0.02 | max. Na₂O |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Spherical Alumina is used in resins, rubbers, and plastics as fillers for thermal conductive sheets, fillers for molding materials, base powder for baking ceramics, blasting materials, and spacers. | |
Color | White, Whitness: 90 | |
Other | Typical Sizing Specifications: Other/Special Sizing is available upon request. Actual PSD & SSA also available upon request. |