General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad aparente | 0.65 - 1.0 g/cm³ Show Supplier Material materials with Densidad aparente of 0.65 - 1.0 g/cm³ | respectively for loose and packed | |
Densidad relativa | 2.42 [-] Show Supplier Material materials with Densidad relativa of 2.42 [-] | ||
Loss on Ignition | 34.6 % Show Supplier Material materials with Loss on Ignition of 34.6 % | at 1000°C | |
Rango de tamaño de partículas | 9.0 µm Show Supplier Material materials with Rango de tamaño de partículas of 9.0 µm | ||
Water content | 105 °C | 0.3 % Show Supplier Material materials with Water content of 0.3 % | |
Área superficial específica | 2.0 m²/g Show Supplier Material materials with Área superficial específica of 2.0 m²/g | BET |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 99.6 % Show Supplier Material materials with Aluminio of 99.6 % | Al(OH)₃ |
Hierro | 0.007 Show Supplier Material materials with Hierro of 0.007 | Fe₂O₃ |
Silicona | 0.005 Show Supplier Material materials with Silicona of 0.005 | SiO₂ |
Sodio | 0.03 Show Supplier Material materials with Sodio of 0.03 | Soluble sodium oxide |
0.24 Show Supplier Material materials with Sodio of 0.24 | Na₂O |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s ATH was developed especially for SMC, BMC, resin injection, and high solids coatings. | |
Other | Screen Analysis: on 325 mesh: 0.1 % through 325 mesh: 99.9 % Less than 10µm: 53% TAPPI Brightness: 89 Oil absorption: 28 ml, boiled linseed oil per 100 gm filler |