General
Property | Temperature | Value | Comment |
---|---|---|---|
Absorción de agua | 25 °C | 25 % Show Supplier Material materials with Absorción de agua of 25 % | min., RH=55%, 24h - Climate Chamber |
Anhydrous Solids Content | 79 % Show Supplier Material materials with Anhydrous Solids Content of 79 % | 1h/800°C | |
85 % Show Supplier Material materials with Anhydrous Solids Content of 85 % | 1h/800°C | ||
Rango de tamaño de partículas | 1.0 - 10.0 µm Show Supplier Material materials with Rango de tamaño de partículas of 1.0 - 10.0 µm | min. 90% | |
Sieve residue 45μm | 0.2 % Show Supplier Material materials with Sieve residue 45μm of 0.2 % | ||
Tamaño de partícula D50 | 3.0 - 5.0 μm Show Supplier Material materials with Tamaño de partícula D50 of 3.0 - 5.0 μm | ||
Tap density | 0.63 g/cm³ Show Supplier Material materials with Tap density of 0.63 g/cm³ | min. | |
Valor de pH | 11.0 - 12.0 [-] Show Supplier Material materials with Valor de pH of 11.0 - 12.0 [-] | 5% Slurry | |
Water content | 18 % Show Supplier Material materials with Water content of 18 % | ||
22 % Show Supplier Material materials with Water content of 22 % |
Óptico
Property | Value | Comment |
---|---|---|
Reflectance | 94.0 [-] Show Supplier Material materials with Reflectance of 94.0 [-] | min., R460 |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 28.0 - 30.0 % Show Supplier Material materials with Aluminio of 28.0 - 30.0 % | Al₂O₃ |
Silicona | 31.0 - 34.0 % Show Supplier Material materials with Silicona of 31.0 - 34.0 % | SiO₂ |
Sodio | 1.5 - 2.5 % Show Supplier Material materials with Sodio of 1.5 - 2.5 % | Na₂SO₄ |
17.0 - 19.0 % Show Supplier Material materials with Sodio of 17.0 - 19.0 % | Na₂O |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Zeolites are used in multiple applications such as detergents, PVC stabilizers, brake pads, water treatment, construction (concrete/ asphalt), agricultre, adsorbents in pharmaceutical & food packaging, manufacture of paints, coatings & paper, as an oder remvoal agent, and many, many more applications. | |
Color | White | |
Other | Calcium Ion Exchange Capacity: Min. 160 mg CaO / g Anhydrous |