General
Property | Value |
---|---|
True particle density | 3.95 g/cm³ Show Supplier Material materials with True particle density of 3.95 g/cm³ |
Mecánica
Property | Value |
---|---|
Dureza (en mohs) | 9.0 [-] Show Supplier Material materials with Dureza (en mohs) of 9.0 [-] |
Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de fusión | 2000.0 °C Show Supplier Material materials with Temperatura de fusión of 2000.0 °C |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 99.78 % Show Supplier Material materials with Aluminio of 99.78 % | Al₂O₃ |
Hierro | 0.09 % Show Supplier Material materials with Hierro of 0.09 % | Fe₂O₃ |
Silicona | 0.04 % Show Supplier Material materials with Silicona of 0.04 % | SiO₂ |
Sodio | 0.1 % Show Supplier Material materials with Sodio of 0.1 % | Na₂O |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s White Aluminum Oxide powders are used for precision lapping, micro blasting, fine grit bond and coated applications, thermal coatings, polishing compounds, and more. | |
Color | White | |
Crystal structure | Alpha-Alumina | |
Other |