General
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.1 Show Supplier Material materials with Aluminio of 0.1 | max. Al₂O₃ |
Calcio | 0.1 % Show Supplier Material materials with Calcio of 0.1 % | CaO |
Circonio | 90 % Show Supplier Material materials with Circonio of 90 % | ZrO₂ |
Hierro | 0.1 Show Supplier Material materials with Hierro of 0.1 | max. Fe₂O₃ |
Itrio | 7.0 - 8.0 % Show Supplier Material materials with Itrio of 7.0 - 8.0 % | Y₂O₃ |
Silicona | 0.4 Show Supplier Material materials with Silicona of 0.4 | max. SiO₂ |
Titanio | 0.1 Show Supplier Material materials with Titanio of 0.1 | max. TiO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Fused Yttria-Stabilized Zirconia is used for refractories, thermal spray coatings, plasma spraying, oxygen permeable membranes, ceramic rings, and many other applications. | |
Color | Yellow | |
Other | Custom Sizing available |