General
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.4 Show Supplier Material materials with Aluminio of 0.4 | max. Al₂O₃ |
Circonio | 94 % Show Supplier Material materials with Circonio of 94 % | min. ZrO₂ |
Hierro | 0.1 Show Supplier Material materials with Hierro of 0.1 | max. Fe₂O₃ |
Magnesio | 3.0 - 4.0 % Show Supplier Material materials with Magnesio of 3.0 - 4.0 % | MgO |
Silicona | 0.4 Show Supplier Material materials with Silicona of 0.4 | max. SiO₂ |
Titanio | 0.2 Show Supplier Material materials with Titanio of 0.2 | max. TiO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Fused MagnesiaStabilized Zirconia is used in various ceramic applications such as refractory setters for the electro-ceramic industry, zirconia furnace furniture, structural ceramics, sizing nozzles, and more. | |
Color | Yellow | |
Other | Custom Sizing available |