General
Property | Value | Comment |
---|---|---|
Rango de tamaño de partículas | 3.0 - 6.0 µm Show Supplier Material materials with Rango de tamaño de partículas of 3.0 - 6.0 µm | |
Área superficial específica | 10.0 Show Supplier Material materials with Área superficial específica of 10.0 | max. |
Chemical properties
Property | Value | Comment |
---|---|---|
Circonio | 99.9 % Show Supplier Material materials with Circonio of 99.9 % | ZrO₂+HfO₂ |
Hierro | 0.003 Show Supplier Material materials with Hierro of 0.003 | max. Fe₂O₃ |
Silicona | 0.015 Show Supplier Material materials with Silicona of 0.015 | max. SiO₂ |
Sodio | 0.003 Show Supplier Material materials with Sodio of 0.003 | max. Na₂O |
Titanio | 0.003 Show Supplier Material materials with Titanio of 0.003 | max. TiO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Chemical Grade Monoclinic Zirconia is used in precision ceramics, electrical components, glass additives, ceramic colored glazes, refractory materials, polishing applications, and synthetic jewelry | |
Color | White | |
Other | SSA & Particle Size can be customized |