General
Property | Value | Comment |
---|---|---|
Loss on Ignition | 1 % Show Supplier Material materials with Loss on Ignition of 1 % | |
Tamaño de partícula D50 | 0.8 Show Supplier Material materials with Tamaño de partícula D50 of 0.8 | max. |
Área superficial específica | 5.0 - 20.0 m²/g Show Supplier Material materials with Área superficial específica of 5.0 - 20.0 m²/g |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.21 - 0.25 % Show Supplier Material materials with Aluminio of 0.21 - 0.25 % | Al₂O₃ |
Circonio | 94 % Show Supplier Material materials with Circonio of 94 % | ZrO₂+HfO₂ |
Hierro | 0.003 Show Supplier Material materials with Hierro of 0.003 | max. Fe₂O₃ |
Itrio | 5.0 - 5.5 % Show Supplier Material materials with Itrio of 5.0 - 5.5 % | Y₂O₃ |
Silicona | 0.02 Show Supplier Material materials with Silicona of 0.02 | max. SiO₂ |
Sodio | 0.005 Show Supplier Material materials with Sodio of 0.005 | max. Na₂O |
Titanio | 0.002 Show Supplier Material materials with Titanio of 0.002 | max. TiO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Chemical Grade Yttria Stabilized Zirconia is used in various ceramic applications where high strength and resistance to wear is necessary. Examples include electrical ceramics, bioceramics, advanced refractory materials, optical fiber components, mechnical parts, cutting tools, oxygen sensors, solid oxide fuel cells, etc. | |
Color | White | |
Other | SSA & Particle Size can be customized |