General
Chemical properties
Property | Value | Comment |
---|---|---|
Circonio | 86 % Show Supplier Material materials with Circonio of 86 % | ZrO₂+HfO₂ |
Hierro | 0.003 Show Supplier Material materials with Hierro of 0.003 | max. Fe₂O₃ |
Itrio | 13.25 - 13.75 % Show Supplier Material materials with Itrio of 13.25 - 13.75 % | Y₂O₃ |
Silicona | 0.05 Show Supplier Material materials with Silicona of 0.05 | max. SiO₂ |
Sodio | 0.005 Show Supplier Material materials with Sodio of 0.005 | max. Na₂O |
Titanio | 0.002 Show Supplier Material materials with Titanio of 0.002 | max. TiO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Chemical Grade Yttria Stabilized Zirconia is used in various ceramic applications where high strength and resistance to wear is necessary. Examples include electrical ceramics, bioceramics, advanced refractory materials, optical fiber components, mechnical parts, cutting tools, oxygen sensors, solid oxide fuel cells, etc. | |
Color | White |