General
Property | Value | Comment |
---|---|---|
Densidad aparente | 1.25 - 1.45 g/cm³ Show Supplier Material materials with Densidad aparente of 1.25 - 1.45 g/cm³ | Hall Meter |
Loss on Ignition | 1.5 % Show Supplier Material materials with Loss on Ignition of 1.5 % | Resistance Furnace |
3 % Show Supplier Material materials with Loss on Ignition of 3 % | Resistance Furnace | |
Área superficial específica | 5.0 - 20.0 m²/g Show Supplier Material materials with Área superficial específica of 5.0 - 20.0 m²/g | BET |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 0.05 Show Supplier Material materials with Aluminio of 0.05 | max. Al₂O₃ unsing SICP | |
Circonio | 96.2 - 96.6 % Show Supplier Material materials with Circonio of 96.2 - 96.6 % | ZrO₂+HfO₂ using XRF | |
Hierro | 0.0025 Show Supplier Material materials with Hierro of 0.0025 | max.Fe₂O₃ using ICP | |
Magnesio | 3.4 - 3.6 % Show Supplier Material materials with Magnesio of 3.4 - 3.6 % | MgO using ICP | |
Silicona | 0.02 Show Supplier Material materials with Silicona of 0.02 | max. SiO₂ using ICP | |
Titanio | 0.0025@max. TiO₂ using ICP |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Chemical Grade Magnesia-Stabilized Zirconia is an ideal material for valve and pump components, bushings and wear sleeves, industrial tool applications, as well as oil and gas down-hole tools. | |
Color | White, Yellow |