General
Property | Value | Comment |
---|---|---|
Densidad aparente | 1.13 g/cm³ Show Supplier Material materials with Densidad aparente of 1.13 g/cm³ | MS2000 Size Analyzer |
Loss on Ignition | 0.17 % Show Supplier Material materials with Loss on Ignition of 0.17 % | Resistance Furnace |
Área superficial específica | 4.0 m²/g Show Supplier Material materials with Área superficial específica of 4.0 m²/g | SSA-3600 BET |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 0.001 Show Supplier Material materials with Aluminio of 0.001 | max. Al₂O₃ using pectrophotometry | |
Circonio | 94.6 - 94.8 % Show Supplier Material materials with Circonio of 94.6 - 94.8 % | ZrO₂+HfO₂ using Bitter Almond Acid Gravimetric Method | |
Hierro | 0.003 Show Supplier Material materials with Hierro of 0.003 | max. Fe₂O₃ using spectrophotometry | |
Magnesio | 2.5 - 2.9 % Show Supplier Material materials with Magnesio of 2.5 - 2.9 % | MgO spectrophotometry | |
Silicona | 0.007 Show Supplier Material materials with Silicona of 0.007 | max. SiO₂ using spectrophotometry | |
Titanio | 0.001@max. TiO₂ using spectrophotometry |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Chemical Grade Magnesia-Stabilized Zirconia is an ideal material for valve and pump components, bushings and wear sleeves, industrial tool applications, as well as oil and gas down-hole tools. | |
Color | White |