General
Property | Value | Comment |
---|---|---|
Densidad aparente | 2.02 - 2.34 g/cm³ Show Supplier Material materials with Densidad aparente of 2.02 - 2.34 g/cm³ | ANSI B74.4 |
Tamaño de los cristales | 12.0 μm Show Supplier Material materials with Tamaño de los cristales of 12.0 μm | |
True particle density | 4.6 g/cm³ Show Supplier Material materials with True particle density of 4.6 g/cm³ |
Mecánica
Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de fusión | 1900.0 °C Show Supplier Material materials with Temperatura de fusión of 1900.0 °C |
Chemical properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Aluminio | 60 % Show Supplier Material materials with Aluminio of 60 % | ANSI B74.14 | max. Al₂O₃ |
Calcio | 0.09 % Show Supplier Material materials with Calcio of 0.09 % | ANSI B74.14 | CaO |
Circonio | 39 % Show Supplier Material materials with Circonio of 39 % | ANSI B74.14 | ZrO₂ |
Hierro | 0.25 % Show Supplier Material materials with Hierro of 0.25 % | ANSI B74.14 | Fe₂O₃ |
Magnesio | 0.02 % Show Supplier Material materials with Magnesio of 0.02 % | ANSI B74.14 | MgO |
Silicona | 0.33 % Show Supplier Material materials with Silicona of 0.33 % | ANSI B74.14 | SiO₂ |
Sodio | 0.03 % Show Supplier Material materials with Sodio of 0.03 % | ANSI B74.14 | Na₂O |
Titanio | 0.25 % Show Supplier Material materials with Titanio of 0.25 % | ANSI B74.14 | TiO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Alumina Zirconia 40% is used for both coated abrasive products and organic bonded grinding wheels. |