General
Property | Value |
---|---|
Densidad | 3.16 g/cm³ Show Supplier Material materials with Densidad of 3.16 g/cm³ |
Porosidad | 6.0 % Show Supplier Material materials with Porosidad of 6.0 % |
Aplicaciones térmicas
Property | Value |
---|---|
Temperatura máx. de funcionamiento | 1700.0 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 1700.0 °C |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 75.0 - 77.0 % Show Supplier Material materials with Aluminio of 75.0 - 77.0 % | Al₂O₃ |
Calcio | 0.05 Show Supplier Material materials with Calcio of 0.05 | max. CaO |
Hierro | 0.1 Show Supplier Material materials with Hierro of 0.1 | max. Fe₂O₃ |
Silicona | 22.5 - 24.5 % Show Supplier Material materials with Silicona of 22.5 - 24.5 % | SiO₂ |
Sodio | 0.1 Show Supplier Material materials with Sodio of 0.1 | max. Na₂O |
Titanio | 0.02 Show Supplier Material materials with Titanio of 0.02 | max. TiO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s White Fused Mullite is used in the investment casting, for producing refractories for the steel industry for the production of high purity mullite blocks for glass melting furnaces, for kiln furniture, and many other applications. | |
Crystal structure | Mullite Phase: 93%, α - Al2O3 Phase: 3%, Glassy Phase: 4% | |
Other | Available sizing: 3-5 mm, 1-3mm, 0.5-1 mm, 0-1 mm, 0-0.5 mm, 0-0.1 mm, 200/F, 325 F Other sizes are available upon request. |