Aplicaciones térmicas
Property | Value |
---|---|
Temperatura máx. de funcionamiento | 1750.0 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 1750.0 °C |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 44.5 - 47.0 % Show Supplier Material materials with Aluminio of 44.5 - 47.0 % | Al₂O₃ |
Circonio | 34.0 - 38.5 % Show Supplier Material materials with Circonio of 34.0 - 38.5 % | ZrO₂ |
Hierro | 0.2 Show Supplier Material materials with Hierro of 0.2 | max. Fe₂O₃ |
Silicona | 16.0 - 18.0 % Show Supplier Material materials with Silicona of 16.0 - 18.0 % | SiO₂ |
Sodio | 0.25 Show Supplier Material materials with Sodio of 0.25 | max. Na₂O |
Titanio | 0.18 Show Supplier Material materials with Titanio of 0.18 | max. TiO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Fused Zirconia Mullite is an excellent material for refractory applications such as glide gates, nozzles, and special refractory parts for the glass industry. | |
Crystal structure | α - Al2O3 Phase: 4% | |
Other | Available sizing: 3-5 mm, 1-3mm, 0.5-1 mm, 0-1 mm, 0-0.5 mm, 0-0.1 mm, 200/F, 325/F Other sizes are available upon request. |