General
Aplicaciones térmicas
Property | Value |
---|---|
Temperatura máx. de funcionamiento | 1900.0 °C Show Supplier Material materials with Temperatura máx. de funcionamiento of 1900.0 °C |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 71.0 - 73.0 % Show Supplier Material materials with Aluminio of 71.0 - 73.0 % | Al₂O₃ |
Calcio | 0.28 Show Supplier Material materials with Calcio of 0.28 | max. CaO |
Hierro | 0.19 Show Supplier Material materials with Hierro of 0.19 | max. Fe₂O₃ |
Magnesio | 26.0 - 28.0 % Show Supplier Material materials with Magnesio of 26.0 - 28.0 % | MgO |
Silicona | 0.1 Show Supplier Material materials with Silicona of 0.1 | max. SiO₂ |
Sodio | 0.18 Show Supplier Material materials with Sodio of 0.18 | max. Na₂O |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s FS27 is used in the production of refractory materials used for the sinter and transit zones of rotary furnaces in the cement industry, for the arches of electric arc furnaces, for the refractory lining of highfrequency furnaces, and various kinds of torpedo ladles and other ladles used in the steel industry. | |
Crystal structure | α - Al2O3 Phase: 1%, Periclase Phase: 0% | |
Other | Available sizing: 3-5 mm, 1-3mm, 0.5-1 mm, 0-1 mm, 0-0.5 mm, 0-0.1 mm, 200/F, 325/F Other sizes are available upon request. |