General
Property | Value | Comment |
---|---|---|
Absorción de agua | 1 % Show Supplier Material materials with Absorción de agua of 1 % | max. |
Densidad | 3.2 g/cm³ Show Supplier Material materials with Densidad of 3.2 g/cm³ | |
Porosidad | 1.2 - 2.6 % Show Supplier Material materials with Porosidad of 1.2 - 2.6 % |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 78 % Show Supplier Material materials with Aluminio of 78 % | Al₂O₃ |
Calcio | 0.2 % Show Supplier Material materials with Calcio of 0.2 % | CaO |
Hierro | 0.15 % Show Supplier Material materials with Hierro of 0.15 % | Fe₂O₃ |
Magnesio | 21.4 % Show Supplier Material materials with Magnesio of 21.4 % | MgO |
Silicona | 0.13 % Show Supplier Material materials with Silicona of 0.13 % | SiO₂ |
Sodio | 0.12 % Show Supplier Material materials with Sodio of 0.12 % | Na₂O |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Sintered MAS is used in the production of refractory materials used for the sinter and transit zones of rotary furnaces in the cement industry, for the arches of electric arc furnaces, for the refractory lining of highfrequency furnaces, and various kinds of torpedo ladles and other ladles used in the steel industry. | |
Other | Available sizing: |