General
Property | Value |
---|---|
True particle density | 5.05 g/cm³ Show Supplier Material materials with True particle density of 5.05 g/cm³ |
Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de fusión | 2410.0 °C Show Supplier Material materials with Temperatura de fusión of 2410.0 °C |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.01 Show Supplier Material materials with Aluminio of 0.01 | max. Al₂O₃ |
Hierro | 0.01 Show Supplier Material materials with Hierro of 0.01 | max. Fe₂O₃ |
Itrio | 99.5 % Show Supplier Material materials with Itrio of 99.5 % | min. Y₂O₃ |
Silicona | 0.02 Show Supplier Material materials with Silicona of 0.02 | max. SiO₂ |
Titanio | 0.01 Show Supplier Material materials with Titanio of 0.01 | max. TiO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Fused Yttrium Oxide is typically used in the titanium casting and specialty ceramics industries. | |
Other | Available Sizing: |