General
Property | Value | Comment |
---|---|---|
Loss on Ignition | 0.1 % Show Supplier Material materials with Loss on Ignition of 0.1 % | max. |
Tamaño de partícula D50 | 1.0 - 40.0 μm Show Supplier Material materials with Tamaño de partícula D50 of 1.0 - 40.0 μm | different specifications, please refer to the table below |
True particle density | 2.15 g/cm³ Show Supplier Material materials with True particle density of 2.15 g/cm³ | |
2.25 g/cm³ Show Supplier Material materials with True particle density of 2.25 g/cm³ |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.15 Show Supplier Material materials with Aluminio of 0.15 | max. Al₂O₃ |
Calcio | 0.008 Show Supplier Material materials with Calcio of 0.008 | max. CaO |
Cloro | 0.0005 Show Supplier Material materials with Cloro of 0.0005 | max. Cl⁻ |
Hierro | 0.0015 Show Supplier Material materials with Hierro of 0.0015 | Fe²⁺ |
0.01 Show Supplier Material materials with Hierro of 0.01 | max. Fe₂O₃ | |
Magnesio | 0.008 Show Supplier Material materials with Magnesio of 0.008 | |
Potasio | 0.008 Show Supplier Material materials with Potasio of 0.008 | max. K₂O |
Silicona | 99.3 % Show Supplier Material materials with Silicona of 99.3 % | min. SiO₂ |
Sodio | 0.0005 Show Supplier Material materials with Sodio of 0.0005 | Na⁺ |
0.01 Show Supplier Material materials with Sodio of 0.01 | max. Na₂O | |
Titanio | 0.008 Show Supplier Material materials with Titanio of 0.008 | max. TiO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Spherical Fused Silica Powder is widely used in various industries such as encapsulation of electronic products and chip material, fiber optic cable, special engineering plastics, rubber, cermic, filler for heat dissipation board (MC board), heat dissipating grease, ink, chemical industry, and many other applications. | |
Other |