General
Property | Value | Comment |
---|---|---|
Densidad aparente | 0.304 g/cm³ Show Supplier Material materials with Densidad aparente of 0.304 g/cm³ | |
Loss on Ignition | 1.7 % Show Supplier Material materials with Loss on Ignition of 1.7 % | max. (970°C/1 hrs) |
Valor de pH | 7.5 [-] Show Supplier Material materials with Valor de pH of 7.5 [-] | |
Water content | 0.3 % Show Supplier Material materials with Water content of 0.3 % | |
Área superficial específica | 20.5 m²/g Show Supplier Material materials with Área superficial específica of 20.5 m²/g | BET |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.11 Show Supplier Material materials with Aluminio of 0.11 | Al₂O₃ |
Azufre | 0.01 % Show Supplier Material materials with Azufre of 0.01 % | SO₂ |
Calcio | 0.42 Show Supplier Material materials with Calcio of 0.42 | max. CaO |
Carbono | 1.1 % Show Supplier Material materials with Carbono of 1.1 % | free carbon |
Cloro | 0.0095 Show Supplier Material materials with Cloro of 0.0095 | |
Hierro | 0.08 Show Supplier Material materials with Hierro of 0.08 | Fe₂O₃ |
Magnesio | 0.29 % Show Supplier Material materials with Magnesio of 0.29 % | |
Potasio | 0.38 Show Supplier Material materials with Potasio of 0.38 | K₂O |
Silicona | 0.12 % Show Supplier Material materials with Silicona of 0.12 % | free silicon |
96 % Show Supplier Material materials with Silicona of 96 % | SiO₂ | |
Sodio | 0.06 % Show Supplier Material materials with Sodio of 0.06 % | Na₂O |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Silica Fume is perfect for use in refractory castables, including low and medium cement, vibratables, and self-flow castables. Use of Silica Fume improves the mechanical properties (MOR, CCS, creep,etc.) of castables by acting as a flow agent of water required to place refractory castable mix. | |
Other | > 45 microns: 2.2 % Brightness: 47 |