General
Property | Value | Comment |
---|---|---|
Absorción de agua | 0 % Show Supplier Material materials with Absorción de agua of 0 % | |
Densidad | 6.0 - 6.08 g/cm³ Show Supplier Material materials with Densidad of 6.0 - 6.08 g/cm³ | packed density: 3.6-3.8 |
Mecánica
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Zirconia Grinding Media is used for audio/video recording tapes, electronic-grade ceramics, ferroelectric, piezoelectric, dielectric, capacitors, sensors, inks, dyes, paint, and other pigments. | |
Color | Milk White | |
Other | Available Sizes: Yttria Stabilized Spheres: Φ0.4, Φ0.5, Φ0.8, Φ1, Φ1.5, Φ2, Φ2.5, Φ3, Φ4, Φ5, Φ7, Φ8, Φ10, Φ12, Φ15, Φ20, Φ25, Φ30 mm Yttria Stabilized Cylinders: 3x3, 5x5, 7x7, 10x10, 12.7x12.7, 15x15, 20x20 mm | |
Wear resistance | Wear Rate (normal): <0.2% , (extreme): <1% |