General
Property | Value |
---|---|
True particle density | 3.95 g/cm³ Show Supplier Material materials with True particle density of 3.95 g/cm³ |
Mecánica
Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de fusión | 2000.0 °C Show Supplier Material materials with Temperatura de fusión of 2000.0 °C |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 95.62 % Show Supplier Material materials with Aluminio of 95.62 % | Al₂O₃ |
Hierro | 0.42 % Show Supplier Material materials with Hierro of 0.42 % | Fe₂O₃ |
Otro | 0.3 Show Supplier Material materials with Otro of 0.3 | |
Silicona | 1.12 % Show Supplier Material materials with Silicona of 1.12 % | SiO₂ |
Titanio | 2.54 Show Supplier Material materials with Titanio of 2.54 | TiO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Brown Aluminum Oxide Macrogrits are used in all types of bonded and coated abrasive applications for ferrous and normal alloy steels. It is also used in a myriad of refractory and general industrial applications. | |
Certifications | ANSI and FEPA Agency & Mil-Specs (such as A-A-59316 & MIL-A-22262B) Pratt & Whitney, Rolls Royce, Praxair, Stryker, etc. | |
Color | Brown | |
Crystal structure | Alpha - Alumina | |
Other |