General
Property | Value |
---|---|
True particle density | 3.95 g/cm³ Show Supplier Material materials with True particle density of 3.95 g/cm³ |
Mecánica
Aplicaciones térmicas
Property | Value |
---|---|
Temperatura de fusión | 2000.0 °C Show Supplier Material materials with Temperatura de fusión of 2000.0 °C |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 98.3 % Show Supplier Material materials with Aluminio of 98.3 % | Al₂O₃ |
Calcio | 0.02 Show Supplier Material materials with Calcio of 0.02 | CaO |
Hierro | 0.04 % Show Supplier Material materials with Hierro of 0.04 % | Fe₂O₃ |
Silicona | 0.04 % Show Supplier Material materials with Silicona of 0.04 % | SiO₂ |
Titanio | 1.58 Show Supplier Material materials with Titanio of 1.58 | TiO₂ |
Technological properties
Property | ||
---|---|---|
Application areas | GNPGraystar’s Semi-Friable Brown Aluminum Oxide is used in all types of bonded and coated abrasive applications for ferrous and normal alloy steels. | |
Certifications | ANSI and FEPA Agency & Mil-Specs (such as A-A-59316 & MIL-A-22262B) Pratt & Whitney, Rolls Royce, Praxair, Stryker, etc. | |
Color | Brown | |
Crystal structure | Alpha - Alumina | |
Other |