Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | The FEPA F grades are especially suitable for the manufacture of vitrified bonded abrasives for working hardened steels and alloys with tensile strengths of over 50 kg/ mm2. These are also used in tool grinding, saw and knife-sharpening applications, precision grinding, profile grinding, flute grinding, tooth grinding, dry grinding of blade segments, and mounted wheels. | |
Color | Ruby | |
Other |