General
Property | Value |
---|---|
Densidad | 3.8 - 4.1 g/cm³ Show Supplier Material materials with Densidad of 3.8 - 4.1 g/cm³ |
Densidad aparente | 2.1 - 2.4 g/cm³ Show Supplier Material materials with Densidad aparente of 2.1 - 2.4 g/cm³ |
Estructura de grano | Sub Angular |
Mecánica
Property | Value |
---|---|
Dureza (en mohs) | 7.5 - 8.0 [-] Show Supplier Material materials with Dureza (en mohs) of 7.5 - 8.0 [-] |
Eléctrico
Property | Value | Comment |
---|---|---|
Conductividad eléctrica | 0.025 Show Supplier Material materials with Conductividad eléctrica of 0.025 | max. |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 18.0 - 20.0 % Show Supplier Material materials with Aluminio of 18.0 - 20.0 % | Al₂O₃ |
Calcio | 10.0 - 11.0 % Show Supplier Material materials with Calcio of 10.0 - 11.0 % | CaO |
Cloro | 0.004 Show Supplier Material materials with Cloro of 0.004 | Sol. Cl |
Hierro | 10.0 - 12.0 % Show Supplier Material materials with Hierro of 10.0 - 12.0 % | Fe₂O₃ |
13.5 - 14.5 % Show Supplier Material materials with Hierro of 13.5 - 14.5 % | Fe₂O | |
Magnesio | 5.5 - 6.5 % Show Supplier Material materials with Magnesio of 5.5 - 6.5 % | |
Manganeso | 0.2 Show Supplier Material materials with Manganeso of 0.2 | max. MnO |
Silicona | 40.0 - 42.0 % Show Supplier Material materials with Silicona of 40.0 - 42.0 % | SiO₂ |
Titanio | 1.5 - 3.5 % Show Supplier Material materials with Titanio of 1.5 - 3.5 % | TiO₂ |
Technological properties
Property | ||
---|---|---|
Certifications | RockRidge Garnet is environmentally inert and meets all Occupational Health and Safety Administration (OSHA) requirements. RockRidge Garnet also meets all ISO 11126-10:200 requirements for chloride and free silica content. | |
Chemical composition | ||
Color | Dark Red / Pink | |
Corrosion properties | Acid Solubility (HCI) < 1.0 % | |
Other | For typical sizings please refer to the pictures on the top right side of the datasheet |