Property | Value | Comment |
---|---|---|
Loss on Ignition | 1 % Show Supplier Material materials with Loss on Ignition of 1 % | max. (1000°C/2 hrs) |
Tamaño de partícula D50 | 2.0 - 10.0 μm Show Supplier Material materials with Tamaño de partícula D50 of 2.0 - 10.0 μm | PSD |
Chemical properties
Property | Value | Comment |
---|---|---|
Calcio | 0.01 Show Supplier Material materials with Calcio of 0.01 | max. CaO |
Cobalto | 0.0002 % Show Supplier Material materials with Cobalto of 0.0002 % | max. Co₃O₄ |
Hierro | 0.001 Show Supplier Material materials with Hierro of 0.001 | max. Fe₂O₃ |
Iterbio | 99.99 % Show Supplier Material materials with Iterbio of 99.99 % | min. Yb₂O₃ |
Níquel | 0.0002 Show Supplier Material materials with Níquel of 0.0002 | max. NiO |
Otro | 0.01 Show Supplier Material materials with Otro of 0.01 | Total Remaining RE-Oxides |
Silicona | 0.01 Show Supplier Material materials with Silicona of 0.01 |
Technological properties
Property | ||
---|---|---|
Application areas | It is typically used as a phosphor activator and in coding material for security systems. |