General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.01 g/cm³ Show Supplier Material materials with Densidad of 1.01 g/cm³ | ISO1183 |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Dureza Shore D | 23.0 °C | 52 - 53 [-] Show Supplier Material materials with Dureza Shore D of 52 - 53 [-] | ISO868 | ||
Módulo de flexión | 23.0 °C | 0.17 GPa Show Supplier Material materials with Módulo de flexión of 0.17 GPa | ISO178 | ||
Resistencia a la tracción | 23.0 °C | 52 MPa Show Supplier Material materials with Resistencia a la tracción of 52 MPa | ISO527 | ||
Resistencia al choque, ensayo Charpy entallado | ISO179, No break @-30, 23°C |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Temperatura de fusión | 158 °C Show Supplier Material materials with Temperatura de fusión of 158 °C | ISO11357 |
Technological properties
Property | ||
---|---|---|
Application areas | Glass frames, eyeglasses frames, eyeglasses, sports sunglasses, watches, headphones, water cups, precipitation cups, filter cups, water-oil separators, fuel filter, filter filters, baby bottles, tea cups, edible oil bottles, cosmetics containers, dashboards, milk machinery shells, eyeglasses, water filter bowls, filter coverage, pneumatic air bowls. |