General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.03 g/cm³ Show Supplier Material materials with Densidad of 1.03 g/cm³ | ISO1183 |
Mecánica
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Dureza Shore D | 23.0 °C | 65 [-] Show Supplier Material materials with Dureza Shore D of 65 [-] | ISO868 | ||
Elongación | 23.0 °C | 100 % Show Supplier Material materials with Elongación of 100 % | ISO527 | ||
Límite elástico | 23.0 °C | 28 MPa Show Supplier Material materials with Límite elástico of 28 MPa | ISO527 | ||
Módulo elástico | 23.0 °C | 0.5 GPa Show Supplier Material materials with Módulo elástico of 0.5 GPa | ISO527 | ||
Resistencia a la tracción | 23.0 °C | 45 MPa Show Supplier Material materials with Resistencia a la tracción of 45 MPa | ISO527 | ||
Resistencia al choque, ensayo Charpy entallado | -30.0 °C | 7 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 7 kJ/m² | ISO179 | ||
23.0 °C | 90 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 90 kJ/m² | ISO179 | |||
Resistencia al choque, ensayo Charpy no entallado | ISO179, No break @-30, 23°C |
Aplicaciones térmicas
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Rigidez dieléctrica | 23.0 °C | 32 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 32 kV/mm | IEC60243-1 |
Volume resistivity | 23.0 °C | 1.00E+14 Ω·cm Show Supplier Material materials with Volume resistivity of 1.00E+14 Ω·cm | IEC60093 |
Índice de seguimiento comparativo | 23.0 °C | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | IEC60112 |
Rheological Properties
Property | Temperature | Value |
---|---|---|
Contracción | 23.0 °C | 0.8 - 1.1 % Show Supplier Material materials with Contracción of 0.8 - 1.1 % |
Technological properties
Property | ||
---|---|---|
Application areas | Tubing, Corrugated pipe | |
Processing methods | Drying Temperature: 80-85°C, Drying Time: 4-6 hr; Rear Temperature: 200°C, Middle Temperature: 210°C, Front Temperature: 220°C, Nozzle Temperature: 230°C |