General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.08 g/cm³ Show Supplier Material materials with Densidad of 1.08 g/cm³ | ISO1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 300 % Show Supplier Material materials with Elongación of 300 % | ISO527 |
Módulo elástico | 23.0 °C | 2.5 GPa Show Supplier Material materials with Módulo elástico of 2.5 GPa | ISO527 |
Resistencia a la tracción | 23.0 °C | 66 MPa Show Supplier Material materials with Resistencia a la tracción of 66 MPa | ISO527 |
Resistencia al choque, ensayo Charpy entallado | -30.0 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6 kJ/m² | ISO179 |
23.0 °C | 10 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10 kJ/m² | ISO179 | |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 1.80 MPa | 68 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 68 °C | ISO75/A |
Temperatura de fusión | 215 °C Show Supplier Material materials with Temperatura de fusión of 215 °C | ISO11357-1 |
Temperatura de transición del vidrio | 60 °C Show Supplier Material materials with Temperatura de transición del vidrio of 60 °C | ISO11357-1 |
Rheological Properties
Property | Temperature | Value |
---|---|---|
Contracción | 23.0 °C | 1.3 - 1.4 % Show Supplier Material materials with Contracción of 1.3 - 1.4 % |
Technological properties
Property | ||
---|---|---|
Application areas | Gears, battery cover, toothbrush wire, industrial brush wire | |
Processing methods | Drying Temperature: 80-85°C, Drying Time: 4-5 hr, Rear Temperature: 215°C, Middle Temperature: 220°C, Front Temperature: 225°C, Nozzle Temperature: 225°C, Mold Temperature: 40-60°C, Injection Pressure: 80-100 MPa |