General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 1.07 g/cm³ Show Supplier Material materials with Densidad of 1.07 g/cm³ | ISO1183 |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 23.0 °C | 200 % Show Supplier Material materials with Elongación of 200 % | ISO527 |
Módulo elástico | 23.0 °C | 2.3 GPa Show Supplier Material materials with Módulo elástico of 2.3 GPa | ISO527 |
Resistencia a la tracción | 23.0 °C | 62 MPa Show Supplier Material materials with Resistencia a la tracción of 62 MPa | ISO527 |
Resistencia al choque, ensayo Charpy entallado | -30.0 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6 kJ/m² | ISO179 |
23.0 °C | 8 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 8 kJ/m² | ISO179 | |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Heat deflection temperature, 1.80 MPa | 65 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 65 °C | ISO75/A |
Temperatura de fusión | 210 °C Show Supplier Material materials with Temperatura de fusión of 210 °C | ISO11357-1 |
Temperatura de transición del vidrio | 60 °C Show Supplier Material materials with Temperatura de transición del vidrio of 60 °C | ISO11357-1 |
Technological properties
Property | ||
---|---|---|
Application areas | Toothbrush wire, industrial brush wire, battery end cap, Gears | |
Processing methods | Drying Temperature: 80-85°C, Drying Time: 4-5 hr, Rear Temperature: 215°C, Middle Temperature: 220°C, Front Temperature: 225°C, Nozzle Temperature: 225°C, Mold Temperature: 60-80°C, Injection Pressure: 80-100 MPa |