General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 14.49 g/cm³ Show Supplier Material materials with Densidad of 14.49 g/cm³ | |
Tamaño de grano | 6 - 10 μm Show Supplier Material materials with Tamaño de grano of 6 - 10 μm | tungsten carbide grain size | |
Tamaño de partícula D90 | 25 μm Show Supplier Material materials with Tamaño de partícula D90 of 25 μm | max |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers 30 | 23.0 °C | 1100 [-] Show Supplier Material materials with Dureza Vickers 30 of 1100 [-] |
Magnético
Property | Temperature | Value |
---|---|---|
Fuerza coercitiva | 23.0 °C | 5174 A/m Show Supplier Material materials with Fuerza coercitiva of 5174 A/m |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 0.02 % Show Supplier Material materials with Aluminio of 0.02 % | max | |
Carbono | as WC balance | ||
Cobalto | 5 - 8 % Show Supplier Material materials with Cobalto of 5 - 8 % | ||
Cobre | 0.02 % Show Supplier Material materials with Cobre of 0.02 % | max | |
Cromo | 0.05 % Show Supplier Material materials with Cromo of 0.05 % | max | |
Hierro | 0.3 % Show Supplier Material materials with Hierro of 0.3 % | max | |
Níquel | 0.1 % Show Supplier Material materials with Níquel of 0.1 % | max | |
Otro | 0.2 % Show Supplier Material materials with Otro of 0.2 % | Ti+Ta+Nb | |
Oxígeno | 0.3 % Show Supplier Material materials with Oxígeno of 0.3 % | max | |
Vanadio | 0.01 % Show Supplier Material materials with Vanadio of 0.01 % | max | |
Wolframio | as WC balance | ||
Zinc | 5E-3 % Show Supplier Material materials with Zinc of 5E-3 % | max |
Technological properties
Property | ||
---|---|---|
Application areas | Powder Grade EC with it’s low cobalt content and extra coarse, very uniform WC grain size distribution is the perfect powder for multiple mining and rock drilling applications. This material requires only short milling in the ready-to-press powder production and offers good sintered properties. |