General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 14.49 g/cm³ Show Supplier Material materials with Densidad of 14.49 g/cm³ | |
Tamaño de grano | 0.8 - 1.3 μm Show Supplier Material materials with Tamaño de grano of 0.8 - 1.3 μm | tungsten carbide grain size | |
Tamaño de partícula D90 | 6 μm Show Supplier Material materials with Tamaño de partícula D90 of 6 μm | max |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers 30 | 23.0 °C | 1600 [-] Show Supplier Material materials with Dureza Vickers 30 of 1600 [-] |
Magnético
Property | Temperature | Value |
---|---|---|
Fuerza coercitiva | 23.0 °C | 20696 A/m Show Supplier Material materials with Fuerza coercitiva of 20696 A/m |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 0.02 % Show Supplier Material materials with Aluminio of 0.02 % | max | |
Carbono | as WC balance | ||
Cobalto | 8 - 12 % Show Supplier Material materials with Cobalto of 8 - 12 % | ||
Cobre | 0.02 % Show Supplier Material materials with Cobre of 0.02 % | max | |
Cromo | 0.6 % Show Supplier Material materials with Cromo of 0.6 % | max | |
Hierro | 0.3 % Show Supplier Material materials with Hierro of 0.3 % | max | |
Niobio | 0.1 % Show Supplier Material materials with Niobio of 0.1 % | max | |
Níquel | 0.1 % Show Supplier Material materials with Níquel of 0.1 % | max | |
Oxígeno | 0.5 % Show Supplier Material materials with Oxígeno of 0.5 % | max | |
Titanio | 0.1 % Show Supplier Material materials with Titanio of 0.1 % | max | |
Tántalo | 0.1 % Show Supplier Material materials with Tántalo of 0.1 % | max | |
Vanadio | 0.2 % Show Supplier Material materials with Vanadio of 0.2 % | max | |
Wolframio | as WC balance | ||
Zinc | 5E-3 % Show Supplier Material materials with Zinc of 5E-3 % | max |
Technological properties
Property | ||
---|---|---|
Application areas | Powder grade F Premium was developed for use in a wide range of tooling products, such as hardmetal rods, indexable inserts, woodworking tools and wear parts. | |
Other | Extremely fine particle sized powder with submicron WC grain size is the optimum solution to applications like extrusion of hard metal rods, knives and others where coarse WC grains are not allowed. When comparing to standard grade F powder, F Premium has a higher shrinkage rate. |