General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 14.49 g/cm³ Show Supplier Material materials with Densidad of 14.49 g/cm³ | |
Tamaño de grano | 0.8 - 1.3 μm Show Supplier Material materials with Tamaño de grano of 0.8 - 1.3 μm | tungsten carbide grain size | |
Tamaño de partícula D90 | 16 μm Show Supplier Material materials with Tamaño de partícula D90 of 16 μm | max |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers 30 | 23.0 °C | 1560 [-] Show Supplier Material materials with Dureza Vickers 30 of 1560 [-] |
Magnético
Property | Temperature | Value |
---|---|---|
Fuerza coercitiva | 23.0 °C | 19104 A/m Show Supplier Material materials with Fuerza coercitiva of 19104 A/m |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 0.02 % Show Supplier Material materials with Aluminio of 0.02 % | max | |
Carbono | as WC balance | ||
Cobalto | 8 - 12 % Show Supplier Material materials with Cobalto of 8 - 12 % | ||
Cobre | 0.02 % Show Supplier Material materials with Cobre of 0.02 % | max | |
Cromo | 0.6 % Show Supplier Material materials with Cromo of 0.6 % | max | |
Hierro | 0.3 % Show Supplier Material materials with Hierro of 0.3 % | max | |
Niobio | 0.1 % Show Supplier Material materials with Niobio of 0.1 % | max | |
Níquel | 0.1 % Show Supplier Material materials with Níquel of 0.1 % | max | |
Oxígeno | 0.3 % Show Supplier Material materials with Oxígeno of 0.3 % | max | |
Titanio | 0.1 % Show Supplier Material materials with Titanio of 0.1 % | max | |
Tántalo | 0.1 % Show Supplier Material materials with Tántalo of 0.1 % | max | |
Vanadio | 0.2 % Show Supplier Material materials with Vanadio of 0.2 % | max | |
Wolframio | as WC balance | ||
Zinc | 5E-3 % Show Supplier Material materials with Zinc of 5E-3 % | max |
Technological properties
Property | ||
---|---|---|
Application areas | Powder grade F was developed for use in a wide range of tooling products, such as hardmetal rods, indexable inserts, woodworking tools and wear parts. | |
Other | Grade F powder exhibits a unifrom WC grain size distribution with evenly distributed WC and Cobalt particles. Thanks to the fine particle size of the powder, milling characteristics are great and comparable to virgin WC-Co powders. |