General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 14.49 g/cm³ Show Supplier Material materials with Densidad of 14.49 g/cm³ | |
Tamaño de grano | 1.3 - 3.5 μm Show Supplier Material materials with Tamaño de grano of 1.3 - 3.5 μm | tungsten carbide grain size | |
Tamaño de partícula D90 | 16 μm Show Supplier Material materials with Tamaño de partícula D90 of 16 μm | max |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers 30 | 23.0 °C | 1360 [-] Show Supplier Material materials with Dureza Vickers 30 of 1360 [-] |
Magnético
Property | Temperature | Value |
---|---|---|
Fuerza coercitiva | 23.0 °C | 9552 A/m Show Supplier Material materials with Fuerza coercitiva of 9552 A/m |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 0.02 % Show Supplier Material materials with Aluminio of 0.02 % | max | |
Carbono | as WC balance | ||
Cobalto | 6 - 20 % Show Supplier Material materials with Cobalto of 6 - 20 % | ||
Cobre | 0.02 % Show Supplier Material materials with Cobre of 0.02 % | max | |
Cromo | 0.2 % Show Supplier Material materials with Cromo of 0.2 % | max | |
Hierro | 0.6 % Show Supplier Material materials with Hierro of 0.6 % | max | |
Níquel | 0.15 % Show Supplier Material materials with Níquel of 0.15 % | max | |
Otro | 0.5 % Show Supplier Material materials with Otro of 0.5 % | Ti+Ta+Nb | |
Oxígeno | 0.3 % Show Supplier Material materials with Oxígeno of 0.3 % | max | |
Vanadio | 0.1 % Show Supplier Material materials with Vanadio of 0.1 % | max | |
Wolframio | as WC balance | ||
Zinc | 5E-3 % Show Supplier Material materials with Zinc of 5E-3 % | max |
Technological properties
Property | ||
---|---|---|
Application areas | Powder grade M was developed for use in a wide range of tooling products, such as indexable inserts, woodworking tools and wear parts. | |
Other | Powder Grade M has evenly distributed WC and Cobalt particles with a fine particle size. Thanks to excellent milling characteristics, the same powder processing parameters can be utilized with Grade M as used with virgin WC-Co powders. |