General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 14.46 g/cm³ Show Supplier Material materials with Densidad of 14.46 g/cm³ | |
Tamaño de grano | 0.5 - 0.8 μm Show Supplier Material materials with Tamaño de grano of 0.5 - 0.8 μm | tungsten carbide grain size | |
Tamaño de partícula D90 | 13 μm Show Supplier Material materials with Tamaño de partícula D90 of 13 μm | max |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers 30 | 23.0 °C | 1630 [-] Show Supplier Material materials with Dureza Vickers 30 of 1630 [-] |
Magnético
Property | Temperature | Value |
---|---|---|
Fuerza coercitiva | 23.0 °C | 21492 A/m Show Supplier Material materials with Fuerza coercitiva of 21492 A/m |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 0.05 % Show Supplier Material materials with Aluminio of 0.05 % | max | |
Carbono | as WC balance | ||
Cobalto | 5 - 8 % Show Supplier Material materials with Cobalto of 5 - 8 % | ||
Cobre | 5E-3 % Show Supplier Material materials with Cobre of 5E-3 % | max | |
Cromo | 0.65 % Show Supplier Material materials with Cromo of 0.65 % | max | |
Hierro | 0.15 % Show Supplier Material materials with Hierro of 0.15 % | max | |
Niobio | 0.1 % Show Supplier Material materials with Niobio of 0.1 % | max | |
Níquel | 0.1 % Show Supplier Material materials with Níquel of 0.1 % | max | |
Oxígeno | 0.35 % Show Supplier Material materials with Oxígeno of 0.35 % | max | |
Titanio | 0.1 % Show Supplier Material materials with Titanio of 0.1 % | max | |
Tántalo | 0.1 % Show Supplier Material materials with Tántalo of 0.1 % | max | |
Vanadio | 0.3 % Show Supplier Material materials with Vanadio of 0.3 % | max | |
Wolframio | as WC balance | ||
Zinc | 5E-3 % Show Supplier Material materials with Zinc of 5E-3 % | max |
Technological properties
Property | ||
---|---|---|
Application areas | Powder grade S was developed for use in a wide range of tooling products, such as hardmetal rods, indexable inserts, woodworking tools and wear parts. | |
Other | Grade S powder has an uniform WC grain size distribution with evenly distributed WC and Cobalt particles. Due to the fine particle size of the powder, milling characteristics are excellent and comparable to virgin WC-Co powders. |