General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 13.24 g/cm³ Show Supplier Material materials with Densidad of 13.24 g/cm³ | |
Tamaño de grano | 1.3 - 3.5 μm Show Supplier Material materials with Tamaño de grano of 1.3 - 3.5 μm | tungsten carbide grain size | |
Tamaño de partícula D90 | 16 μm Show Supplier Material materials with Tamaño de partícula D90 of 16 μm | max |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers 30 | 23.0 °C | 1145 [-] Show Supplier Material materials with Dureza Vickers 30 of 1145 [-] |
Magnético
Property | Temperature | Value |
---|---|---|
Fuerza coercitiva | 23.0 °C | 10188 A/m Show Supplier Material materials with Fuerza coercitiva of 10188 A/m |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 0.05 % Show Supplier Material materials with Aluminio of 0.05 % | max | |
Carbono | as WC balance | ||
Cobalto | 7 - 12 % Show Supplier Material materials with Cobalto of 7 - 12 % | ||
Cobre | 0.05 % Show Supplier Material materials with Cobre of 0.05 % | max | |
Cromo | 0.2 % Show Supplier Material materials with Cromo of 0.2 % | max | |
Hierro | 0.5 % Show Supplier Material materials with Hierro of 0.5 % | max | |
Niobio | 0.3 % Show Supplier Material materials with Niobio of 0.3 % | max | |
Níquel | 0.5 % Show Supplier Material materials with Níquel of 0.5 % | max | |
Oxígeno | 0.3 % Show Supplier Material materials with Oxígeno of 0.3 % | max | |
Titanio | 0.5 % Show Supplier Material materials with Titanio of 0.5 % | max | |
Tántalo | 0.7 % Show Supplier Material materials with Tántalo of 0.7 % | max | |
Vanadio | 0.07 % Show Supplier Material materials with Vanadio of 0.07 % | max | |
Wolframio | as WC balance | ||
Zinc | 5E-3 % Show Supplier Material materials with Zinc of 5E-3 % | max |
Technological properties
Property | ||
---|---|---|
Application areas | Powder grade TS was developed for use in a wide range of tooling products, such as indexable inserts, woodworking tools and wear parts. | |