Material: el 'StarCeram® S Sintered Silicon Carbide (SSiC)' que buscabas ha sido remplazado por el material siguiente.

Pressureless Sintered Silicon Carbide

Want to keep this datasheet? Save it now in your required format

Description

Silicon carbide, mainly consisting of SiC, it maintains strength up to 1400°C and it is ideal for use as a construction material. SiC has excellent thermal conductivity, low thermal expansion and is very resistant to acids and lyes. It masters corrosion, abrasion and erosion as skillfully as it stands up to frictional wear.

Los datos sobre este material han sido proporcionados por Innovacera.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValue

Densidad

23.0 °C

3.13 g/cm³

Show Supplier Material materials with Densidad of 3.13 g/cm³

Mecánica

PropertyTemperatureValue

Dureza Vickers

23.0 °C

2244 [-]

Show Supplier Material materials with Dureza Vickers of 2244 [-]

Módulo elástico

23.0 °C

420 GPa

Show Supplier Material materials with Módulo elástico of 420 GPa

Resistencia a la compresión

23.0 °C

400 MPa

Show Supplier Material materials with Resistencia a la compresión of 400 MPa

Aplicaciones térmicas

PropertyTemperatureValue

Conductividad térmica

23.0 °C

74 W/(m·K)

Show Supplier Material materials with Conductividad térmica of 74 W/(m·K)

Technological properties

Property
Application areas

It is widely used in mechanical seals, seal ring, bearing, pump parts, ballistics, chemical production, energy technology, paper manufacturing and as pipe system components.

Processing methods

pressureless sintering, reaction-bonded sintering, recrystallization sintering