General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 2.65 - 2.75 g/cm³ Show Supplier Material materials with Densidad of 2.65 - 2.75 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Módulo elástico | 23.0 °C | 300 GPa Show Supplier Material materials with Módulo elástico of 300 GPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 4.69E-6 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 4.69E-6 1/K |
Conductividad térmica | 23.0 °C | 36.6 W/(m·K) Show Supplier Material materials with Conductividad térmica of 36.6 W/(m·K) |
Technological properties
Property | ||
---|---|---|
Application areas | It is widely used in mechanical seals, seal ring, bearing, pump parts, ballistics, chemical production, energy technology, paper manufacturing and as pipe system components. | |
Processing methods | pressureless sintering, reaction-bonded sintering, recrystallization sintering |