General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 4.01 g/cm³ Show Supplier Material materials with Densidad of 4.01 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.23 [-] Show Supplier Material materials with Coeficiente de Poisson of 0.23 [-] |
Dureza Vickers | 23.0 °C | 1632 [-] Show Supplier Material materials with Dureza Vickers of 1632 [-] |
Módulo elástico | 23.0 °C | 337 GPa Show Supplier Material materials with Módulo elástico of 337 GPa |
Resistencia a la compresión | 23.0 °C | 2500 MPa Show Supplier Material materials with Resistencia a la compresión of 2500 MPa |
Resistencia a la flexión | 23.0 °C | 300 MPa Show Supplier Material materials with Resistencia a la flexión of 300 MPa |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Calor específico | 23.0 °C | 460 J/(kg·K) Show Supplier Material materials with Calor específico of 460 J/(kg·K) |
Coeficiente de dilatación térmica | 23.0 °C | 8.4E-6 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 8.4E-6 1/K |
Conductividad térmica | 23.0 °C | 14 W/(m·K) Show Supplier Material materials with Conductividad térmica of 14 W/(m·K) |
Eléctrico
Property | Temperature | Value |
---|---|---|
Constante dieléctrica | 23.0 °C | 10 [-] Show Supplier Material materials with Constante dieléctrica of 10 [-] |
Technological properties
Property | ||
---|---|---|
Application areas | Ceramic Valve components, Ceramic Pump liners, Ceramic Roller, Ceramic Plugs, Ceramic Sleeves, Ceramic Pistons, Ceramic Nozzle, Ceramic balls, Ceramic Spools, Ceramic Shaft, Ceramic Press tooling | |
Processing methods | Low Pressure Injection Molding, Cold Isostatic Press, Dry Press, Precision Machining Processing |