Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materiales
Categories
No estás conectado
Categories
Encontrar proveedores de metales
List Your Company
Case Studies
Tools
Sobre nosotros
Los datos sobre este material han sido proporcionados por Heraeus.
All categories
General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 20.7 g/cm³ Show Supplier Material materials with Densidad of 20.7 g/cm³ |
Medidas
Property | Value |
---|---|
Dimensions | Dimensions available upon request. |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers | 23.0 °C | 200 - 550 [-] Show Supplier Material materials with Dureza Vickers of 200 - 550 [-] |
Technological properties
Property | ||
---|---|---|
Application areas | Spark plugs | |
Corrosion properties | Corrosion resistant | |
Other | Erosion resistant, temperature stable |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
EMPRESA
CONTÁCTANOS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.