General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 20 g/cm³ Show Supplier Material materials with Densidad of 20 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Vickers | 23.0 °C | 94 [-] Show Supplier Material materials with Dureza Vickers of 94 [-] | |
Elongación | 20.0 °C | 38 % Show Supplier Material materials with Elongación of 38 % | |
1200.0 °C | 42 % Show Supplier Material materials with Elongación of 42 % | ||
1400.0 °C | 30 % Show Supplier Material materials with Elongación of 30 % | ||
1600.0 °C | 54 % Show Supplier Material materials with Elongación of 54 % | ||
Límite elástico Rp 0,2 | 20.0 °C | 134 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 134 MPa | |
1200.0 °C | 44.3 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 44.3 MPa | ||
1400.0 °C | 27.7 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 27.7 MPa | ||
1600.0 °C | 14.7 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 14.7 MPa | ||
Módulo elástico | 23.0 °C | 213 GPa Show Supplier Material materials with Módulo elástico of 213 GPa | |
Norton Exponent | 1200.0 °C | 3.6 [-] Show Supplier Material materials with Norton Exponent of 3.6 [-] | |
1400.0 °C | 3.6 [-] Show Supplier Material materials with Norton Exponent of 3.6 [-] | ||
1600.0 °C | 3.8 [-] Show Supplier Material materials with Norton Exponent of 3.8 [-] | ||
Resistencia a la fluencia | 1200.0 °C | 2.4 MPa Show Supplier Material materials with Resistencia a la fluencia of 2.4 MPa | 10,000 h (extrapolated data) |
1400.0 °C | 1.3 MPa Show Supplier Material materials with Resistencia a la fluencia of 1.3 MPa | 10,000 h (extrapolated data) | |
1600.0 °C | 0.5 MPa Show Supplier Material materials with Resistencia a la fluencia of 0.5 MPa | 10,000 h (extrapolated data) | |
Resistencia a la tracción | 20.0 °C | 301 MPa Show Supplier Material materials with Resistencia a la tracción of 301 MPa | |
1200.0 °C | 58.8 MPa Show Supplier Material materials with Resistencia a la tracción of 58.8 MPa | ||
1400.0 °C | 35.4 MPa Show Supplier Material materials with Resistencia a la tracción of 35.4 MPa | ||
1600.0 °C | 16.7 MPa Show Supplier Material materials with Resistencia a la tracción of 16.7 MPa | ||
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Conductividad térmica | 20.0 °C | 40.1 W/(m·K) Show Supplier Material materials with Conductividad térmica of 40.1 W/(m·K) |
1200.0 °C | 70.6 W/(m·K) Show Supplier Material materials with Conductividad térmica of 70.6 W/(m·K) | |
1400.0 °C | 70.8 W/(m·K) Show Supplier Material materials with Conductividad térmica of 70.8 W/(m·K) | |
Temperatura de fusión | 1840 - 1870 °C Show Supplier Material materials with Temperatura de fusión of 1840 - 1870 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 2.1E-7 Ω·m Show Supplier Material materials with Resistividad eléctrica of 2.1E-7 Ω·m |
1153.0 °C | 5.3E-7 Ω·m Show Supplier Material materials with Resistividad eléctrica of 5.3E-7 Ω·m | |
1400.0 °C | 5.9E-7 Ω·m Show Supplier Material materials with Resistividad eléctrica of 5.9E-7 Ω·m | |