General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 21.45 g/cm³ Show Supplier Material materials with Densidad of 21.45 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Vickers | 23.0 °C | 42 [-] Show Supplier Material materials with Dureza Vickers of 42 [-] |
Elongación | 20.0 °C | 23 % Show Supplier Material materials with Elongación of 23 % |
1200.0 °C | 64 % Show Supplier Material materials with Elongación of 64 % | |
1400.0 °C | 68 % Show Supplier Material materials with Elongación of 68 % | |
1600.0 °C | 64 % Show Supplier Material materials with Elongación of 64 % | |
Límite elástico Rp 0,2 | 20.0 °C | 59 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 59 MPa |
1200.0 °C | 7.6 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 7.6 MPa | |
1400.0 °C | 3.9 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 3.9 MPa | |
1600.0 °C | 3 MPa Show Supplier Material materials with Límite elástico Rp 0,2 of 3 MPa | |
Módulo elástico | 20.0 °C | 165 GPa Show Supplier Material materials with Módulo elástico of 165 GPa |
1600.0 °C | 60 GPa Show Supplier Material materials with Módulo elástico of 60 GPa | |
Resistencia a la tracción | 20.0 °C | 128 MPa Show Supplier Material materials with Resistencia a la tracción of 128 MPa |
1200.0 °C | 15.6 MPa Show Supplier Material materials with Resistencia a la tracción of 15.6 MPa | |
1400.0 °C | 8.2 MPa Show Supplier Material materials with Resistencia a la tracción of 8.2 MPa | |
1600.0 °C | 4.4 MPa Show Supplier Material materials with Resistencia a la tracción of 4.4 MPa | |
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Conductividad térmica | 20.0 °C | 69.11 W/(m·K) Show Supplier Material materials with Conductividad térmica of 69.11 W/(m·K) |
1200.0 °C | 88.02 W/(m·K) Show Supplier Material materials with Conductividad térmica of 88.02 W/(m·K) | |
1400.0 °C | 90.59 W/(m·K) Show Supplier Material materials with Conductividad térmica of 90.59 W/(m·K) | |
Temperatura de fusión | 1769 °C Show Supplier Material materials with Temperatura de fusión of 1769 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 9.83E-8 Ω·m Show Supplier Material materials with Resistividad eléctrica of 9.83E-8 Ω·m |
1200.0 °C | 4.85E-7 Ω·m Show Supplier Material materials with Resistividad eléctrica of 4.85E-7 Ω·m | |
1400.0 °C | 5.33E-7 Ω·m Show Supplier Material materials with Resistividad eléctrica of 5.33E-7 Ω·m | |