Medidas
Property | Value |
---|---|
Dimensions | Flat wire: Width: 1-12 mm, Thickness: 0.1-2.5 mm |
Mecánica
Aplicaciones térmicas
Property | Temperature | Value |
---|---|---|
Conductividad térmica | 23.0 °C | 90.9 - 91 W/(m·K) Show Supplier Material materials with Conductividad térmica of 90.9 - 91 W/(m·K) |
Recrystallization temperature | 350 °C Show Supplier Material materials with Recrystallization temperature of 350 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 23.0 °C | 7.1E-8 Ω·m Show Supplier Material materials with Resistividad eléctrica of 7.1E-8 Ω·m |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Flat wire: contact in batteries and electronic applications, batteries managment devices, laser ribbon bonding, ultrasonic ribbon bonding | |
Heat Treatment | Soft Annealed | |
Processing history | Ribbon of high purity nickel is produced by two processing routes: I. slitting of strip: thick coil is rolled down on a modren Bühler reversing to the required thickness. The strip is cut on a high precision slitting line. The minimum band width is 1.0 mm. II. Flat rolling of wire: wire is flat rolled using Bühler flat rolling mill to the thickness between 0.10 to 2.5 mm and width between 1.0 and 12.0 mm. | |
Surface Finish | Blank/Bare surface |